描述
PA66+30%玻璃纤维颗粒
PA66+30%玻璃纤维颗粒
PP GF30、PA6 GF30、PA66 FR V0颗粒、
TPU POM PC PP ABS PEI PEEK树脂塑料,
任何颜色都可用,
优点高抗冲击性,易于成型,
玻璃纤维增强碳纤维增强,
阻燃级、增韧级,
包装25kg/袋(也可定制)
PA66+30%玻璃纤维颗粒
产品详细信息
材质 | PA66+30%玻璃纤维颗粒Modle | 由于玻璃纤维在注射成型过程中沿流动方向定向,机械性能和收缩率将在定向方向上增加,导致产品变形和翘曲。因此,在设计模具时,浇口的位置和形状应合理,并可改进工艺。调整模具温度,取出后放入热水中,慢慢冷却 此外,添加的玻璃纤维比例越大,注塑机塑化部件的磨损越大,并且使用了双金属螺杆和筒体 立即联系:特蕾西 PA66+30% Glass Fiber ParticlePA66+30% glass fiber particle PA66+30% Glass Fiber Particle Product Details
PA66+30% glass fiber particle30% glass fiber is added to PA 66, the mechanical properties, dimensional stability, heat resistance, and aging resistance of PA66 are significantly improved, and the fatigue strength is 2.5 times that of unreinforced. The molding process of glass fiber reinforced PA66 is roughly the same as that of the unreinforced PA66, but because the flow is worse than before reinforcement, the injection pressure and injection speed should be appropriately increased, and the barrel temperature should be increased by 10-40°C. Since the glass fiber is oriented along the flow direction during the injection molding process, the mechanical properties and shrinkage rate will increase in the orientation direction, resulting in deformation and warpage of the product. Therefore, when designing the mold, the position and shape of the gate should be reasonable, and the process can be improved. The temperature of the mold, put the product in hot water after taking it out, and let it cool down slowly. In addition, the greater the proportion of glass fiber added, the greater the wear on the plasticizing components of the injection molding machine, and the bimetallic screw and barrel are used. More detail of PA66+30% glass fiber particle.Any interested in, please kindly contact me. Contact now:Tracy<###> 您必须登录才能发表评价。 |
评价
目前还没有评价